All glass must be annealed, or slowly cooled, after it has been made. The annealing process allows the atomic structure of glass relaxes as it cools and thus reduces internal streses that can otherwise weaken the glass. In most cases, annealing is achieved by holding the glass at approximately 5° C (9° F) above its annealing point for 5 to 15 minutes, followed by slowly cooling it through the glass-transition range and the strain point and finally to room temperature. Some glasses, such as [http://cameo.mfa.org/materials/fullrecord.asp?name=tempered%20glass tempered glass], are strengthened by flash cooling the glass from its annealing point. Optical glasses are held for a long-time at their annealing point then so slowly cooled that they have almost no detectable internal stresses.
+
All glass must be annealed, or slowly cooled, after it has been made. The annealing process allows the atomic structure of glass relaxes as it cools and thus reduces internal streses that can otherwise weaken the glass. In most cases, annealing is achieved by holding the glass at approximately 5° C (9° F) above its annealing point for 5 to 15 minutes, followed by slowly cooling it through the glass-transition range and the strain point and finally to room temperature. Some glasses, such as [[tempered%20glass|tempered glass]], are strengthened by flash cooling the glass from its annealing point. Optical glasses are held for a long-time at their annealing point then so slowly cooled that they have almost no detectable internal stresses.
  
 
== Synonyms and Related Terms ==
 
== Synonyms and Related Terms ==

Revision as of 14:09, 7 January 2014

Description

All glass must be annealed, or slowly cooled, after it has been made. The annealing process allows the atomic structure of glass relaxes as it cools and thus reduces internal streses that can otherwise weaken the glass. In most cases, annealing is achieved by holding the glass at approximately 5° C (9° F) above its annealing point for 5 to 15 minutes, followed by slowly cooling it through the glass-transition range and the strain point and finally to room temperature. Some glasses, such as Tempered glass, are strengthened by flash cooling the glass from its annealing point. Optical glasses are held for a long-time at their annealing point then so slowly cooled that they have almost no detectable internal stresses.

Synonyms and Related Terms

tempered glass; heat-strengthened glass

Authority

  • Encyclopedia Britannica, http://www.britannica.com Comment: Glass. Retrieved June 6, 2003, from Encyclopædia Britannica Premium Service.
  • Dictionary of Building Preservation, Ward Bucher, ed., John Wiley & Sons, Inc., New York City, 1996

Retrieved from "https://cameo.mfa.org/index.php?title=Annealed_glass&oldid=42775"