| 366 | | 366 | ||
|- | |- | ||
− | ! scope="row"| | + | ! scope="row"|Uemura number / title |
− | | | + | | ; "Haze-some 25" |
|- | |- | ||
! scope="row"|Folder location | ! scope="row"|Folder location | ||
Line 41: | Line 41: | ||
| - | | - | ||
|- | |- | ||
− | ! scope="row"| | + | ! scope="row"|Uemura's notes |
| 5g of air dried bark of the plant were boiled in 100cc of water, from which 25cc was used for the dyeing. The amount of the contained bark in the dye bath was 2.5 times as much as the weight of the silk used (0.5g). From the right sample, the dye compound were re-extracted from the fabric in a hot water, and the extract was dried. The dried extract weighed 25% of the fabric. | | 5g of air dried bark of the plant were boiled in 100cc of water, from which 25cc was used for the dyeing. The amount of the contained bark in the dye bath was 2.5 times as much as the weight of the silk used (0.5g). From the right sample, the dye compound were re-extracted from the fabric in a hot water, and the extract was dried. The dried extract weighed 25% of the fabric. | ||
|- | |- | ||
− | ! scope="row"| | + | ! scope="row"|Uemura's date |
| Kyoto | | Kyoto | ||
|} | |} | ||
− | [[Category: | + | [[Category:Uemura dye archive]] |
Latest revision as of 19:52, 23 June 2020
Museum number | 366 |
---|---|
Uemura number / title | ; "Haze-some 25" |
Folder location | 5th shelf |
Sample location | right (366 R) |
Fiber type | silk |
Color | red brown |
Dyestuff (Japanese common name) | 相思樹 : Soshijyu |
Dyestuff (botanical name) | Acacia confusa Merr. |
Plant part | bark / air dried |
Dyestuff extraction | boiled in water |
Auxiliary agent in dye bath | - |
Mordant | lime |
Other auxiliary agent | - |
Uemura's notes | 5g of air dried bark of the plant were boiled in 100cc of water, from which 25cc was used for the dyeing. The amount of the contained bark in the dye bath was 2.5 times as much as the weight of the silk used (0.5g). From the right sample, the dye compound were re-extracted from the fabric in a hot water, and the extract was dried. The dried extract weighed 25% of the fabric. |
Uemura's date | Kyoto |