[Martin A Carbone, Inc, Santa Barbara, CA] A trademark for a two-part epoxy putty. Gapoxio (TM) epoxy resin contains mixed diglycidyl ethers of Bisphenol A that is mixed with an amine hardener. Fillers include clay, silica, lime and magnesia. Gapoxio (TM) has a working time of about 45 minutes after kneading equal parts of the A and B sticks. It cures in about an hour at room temperature with no shrinkage. Gapoxio (TM) has a light beige-gray color but dry pigments can be added during mixing for other variations. After cure, the solid resin can be drilled, sanded, cut or painted.
 
[Martin A Carbone, Inc, Santa Barbara, CA] A trademark for a two-part epoxy putty. Gapoxio (TM) epoxy resin contains mixed diglycidyl ethers of Bisphenol A that is mixed with an amine hardener. Fillers include clay, silica, lime and magnesia. Gapoxio (TM) has a working time of about 45 minutes after kneading equal parts of the A and B sticks. It cures in about an hour at room temperature with no shrinkage. Gapoxio (TM) has a light beige-gray color but dry pigments can be added during mixing for other variations. After cure, the solid resin can be drilled, sanded, cut or painted.
  
== Other Properties ==
+
As of 2022, GAPOXIO is no longer being produced.  The replacement for Gapoxio is A + B Putty
  
Smooths with water, alcohol, acetone prior to cure.  Insoluble after cure.  Cleans with soap and water prior to cure.  Cure is shortened with heat or by placing in a microwave oven.
+
==Physical and Chemical Properties==
  
{| class="wikitable"
+
* Smooths with water, alcohol, acetone prior to cure. 
|-
+
* Insoluble after cure. 
! scope="row"| Density
+
* Cleans with soap and water prior to cure. 
| 1.95
+
* Cure time is shortened with heat or by placing in a microwave oven.
|}
+
* Density = 1.95
  
== Hazards and Safety ==
+
== Risks ==
  
 
Contact may cause sensitivity or irritation.
 
Contact may cause sensitivity or irritation.
  
== Additional Information ==
+
==Resources and Citations==
 +
* Rezolin: [http://www.aplusbputty.com/ A+B putty]
  
Gapoxio: [http://www.papershops.com/gapoxio.htm Website]
+
* Gapoxio: [http://www.papershops.com/gapoxio.htm Website]
  
== Authority ==
+
* John Griswold: Contributed information (2002)
  
* External source or communication  Comment: Contributed information (2002): - John Griswold
 
 
* Website address 1  Comment: www.gapoxio.com
 
  
  
  
 
[[Category:Materials database]]
 
[[Category:Materials database]]

Latest revision as of 14:44, 26 August 2022

Description

[Martin A Carbone, Inc, Santa Barbara, CA] A trademark for a two-part epoxy putty. Gapoxio (TM) epoxy resin contains mixed diglycidyl ethers of Bisphenol A that is mixed with an amine hardener. Fillers include clay, silica, lime and magnesia. Gapoxio (TM) has a working time of about 45 minutes after kneading equal parts of the A and B sticks. It cures in about an hour at room temperature with no shrinkage. Gapoxio (TM) has a light beige-gray color but dry pigments can be added during mixing for other variations. After cure, the solid resin can be drilled, sanded, cut or painted.

As of 2022, GAPOXIO is no longer being produced. The replacement for Gapoxio is A + B Putty

Physical and Chemical Properties

  • Smooths with water, alcohol, acetone prior to cure.
  • Insoluble after cure.
  • Cleans with soap and water prior to cure.
  • Cure time is shortened with heat or by placing in a microwave oven.
  • Density = 1.95

Risks

Contact may cause sensitivity or irritation.