Difference between revisions of "Lead alloys"
Jump to navigation
Jump to search
(username removed) |
|||
(2 intermediate revisions by 2 users not shown) | |||
Line 1: | Line 1: | ||
− | [[File:52.1396-C31611CR-d1.jpg|thumb|]] | + | [[File:52.1396-C31611CR-d1.jpg|thumb|Lead-tin alloy inlay<br>MFA# 52.1396]] |
== Description == | == Description == | ||
− | Lead alloys well with other metals and is often used in mixtures containing 62-95% [ | + | Lead alloys well with other metals and is often used in mixtures containing 62-95% [[lead]], 1-35% [[tin]], and 3-13% [[antimony]]. Lead alloys melt at 290-390 C to form a medium viscosity liquid. Lead alloys are soft and do not reproduce fine detail well when molded. |
== Synonyms and Related Terms == | == Synonyms and Related Terms == | ||
Line 8: | Line 8: | ||
alliages de plomb (Fr.); Bleilegierungen (Deut.); aleaciones de plomo (Esp.); lood legering (Ned.); ligas de chumbo (Port.) | alliages de plomb (Fr.); Bleilegierungen (Deut.); aleaciones de plomo (Esp.); lood legering (Ned.); ligas de chumbo (Port.) | ||
− | == | + | == Risks == |
Inhalation and ingestion of lead fumes and dust is very toxic. | Inhalation and ingestion of lead fumes and dust is very toxic. | ||
− | == | + | ==Resources and Citations== |
* David Matthews, Moldmaking and Casting FAQ, www.sfcmd.com/heavygear/faqs/moldmaking_faq.txt | * David Matthews, Moldmaking and Casting FAQ, www.sfcmd.com/heavygear/faqs/moldmaking_faq.txt |
Latest revision as of 09:01, 16 September 2022
Description
Lead alloys well with other metals and is often used in mixtures containing 62-95% Lead, 1-35% Tin, and 3-13% Antimony. Lead alloys melt at 290-390 C to form a medium viscosity liquid. Lead alloys are soft and do not reproduce fine detail well when molded.
Synonyms and Related Terms
alliages de plomb (Fr.); Bleilegierungen (Deut.); aleaciones de plomo (Esp.); lood legering (Ned.); ligas de chumbo (Port.)
Risks
Inhalation and ingestion of lead fumes and dust is very toxic.