Nylon 6T: Difference between revisions

From CAMEO
Jump to navigation Jump to search
m (Text replace - "\[http:\/\/cameo\.mfa\.org\/materials\/fullrecord\.asp\?name=([^\s]+)\s(.*)\]" to "$2")
No edit summary
Line 21: Line 21:
| 1.21
| 1.21
|}
|}
== Additional Information ==
° M. Joseph, ''Introductory Textile Science'', Holt Reinhold & Winston, Fort Worth, 1986, p. 135. ° G.Cook, ''Handbook of Textile Fibres:II. Man-made Fibres'', 5th edition, Merrow Publishing Co., Durham, England, 1984, p.324.


== Sources Checked for Data in Record ==
== Sources Checked for Data in Record ==


* Marjory L. Joseph, ''Introductory Textile Science'', Holt, Rinehart and Winston, Fort Worth, TX, 1986
* Marjory L. Joseph, ''Introductory Textile Science'', Holt, Rinehart and Winston, Fort Worth, TX, 1986, p. 135.


* J.Gordon Cook, ''Handbook of Textile Fibres:II Man-made Fibres'', Merrow Publishing Co. , Durham, England
* J.Gordon Cook, ''Handbook of Textile Fibres:II Man-made Fibres'', Merrow Publishing Co. , Durham, England, 1984, p.324.






[[Category:Materials database]]
[[Category:Materials database]]

Revision as of 19:23, 20 May 2020

Description

Nylon 6T is made by polymerizing hexamethylene diamine with terephthalic acid. Nylon 6T is similar in most properties to nylon 6 and 6,6, but it has a higher melting point and greater density. Nylon 6T also has good heat resistance and resistance to stretch. It is most often used as a precursor for producing aramid fibers.

See nylon fiber.

Synonyms and Related Terms

polyhexamethylene terephthalamide

Other Properties

Moisture regain = 4.5%

Melting Point 370
Density 1.21

Sources Checked for Data in Record

  • Marjory L. Joseph, Introductory Textile Science, Holt, Rinehart and Winston, Fort Worth, TX, 1986, p. 135.
  • J.Gordon Cook, Handbook of Textile Fibres:II Man-made Fibres, Merrow Publishing Co. , Durham, England, 1984, p.324.